Automatic Relaxation and Creep Tester

EB 18-II-3 – Automatic Relaxation & Creep Testing System for Standards-Compliant Long-Term Testing

The EB 18-II-3 is a highly advanced automated testing system designed for performing stress relaxation and creep tests on rubber and plastic materials. With individually controlled stations and temperature zones, it allows for precise, long-term material analysis – standards-compliant and highly configurable.

1. Standards & Temperature Range

✅ Individually controlled temperature and test station settings
✅ Temperature range: +40 °C to +200 °C
✅ Conforms to the following standards:

 

2. Key Features & Equipment

🔹 Standard Configuration

✅ Includes compression plates and 1000 N load cells
✅ Expandable with accessories for specific test applications:

🔹 Available Versions

✅ EB 18-II-3HT – high-temperature version up to +300 °C
✅ EB 18-II-3HF – high-force version up to 2000 N

🔹 Testing at Room Temperature

✅ Easily possible by raising the test stations inside the hood

 

3. Modern Design & Control

✅ Servo-motorized control system – enables precise lowering, lifting, compression, and extension
✅ Polycarbonate housing with aluminum frame – ensures outstanding thermal stability
✅ Integrated high-precision aging oven – compliant with ISO 188 Method A

 

4. EC 13 Control Software

✅ Windows-based application for:

 

5. Quick Switching Between Test Modes

✅ Same accessories used for both stress relaxation and creep testing
✅ Test mode selection directly in the EC 13 software
✅ Fast conversion between tension and compression with easy rig reconfiguration (detailed in the manual)

📌 Recommendation: For best performance, the unit should be operated in an environment with a stable ambient temperature between +10 °C and +30 °C.

 

With the EB 18-II-3, you gain a fully automated, high-precision, and versatile test system for long-term mechanical testing – ideal for laboratories, development, and quality control.

📞 Contact us for more information!

Specifications:

Standards:

  • ISO 188 Method A
  • ISO 3384-1 Method A
  • ISO 6914 Method A
  • ISO 899 with modification
  • other equivalent standards

Temperature range:

+40 °C to +200 °C (EB 18-II-3, EB 18-II-3HF)

+40 °C to +300 °C (EB 18-II-3HT)

Included in the scope of delivery:

  • All-in-one computer (Windows) with monitor, keyboard and mouse
  • First year support contract
  • Manual in English
  • Tools such as a stylus pen for the instrument's touchscreen
  • Accredited calibration incl. certificate

Important specifications:

  • EC 13 Software - Required for the use of EB 18-II-3
  • Temperature fluctuation in time ± 0.25 °C
  • Temperature display with sensor in each cell (PLC)
  • Temperature controller with 0.1°C setpoint (PLC)
  • Adjustable upper and lower temperature limits with alarm (PLC)
  • Control via a micro PLC with colour touchscreen
  • Test names can be specified in the PLC
  • Special version with controlled air exchange rate and low air speed
  • Built-in air pump
  • Low air pressure alarm (PLC)
  • Improved insulation reduces energy consumption, environmental impact and costs
  • Cooling ducts in the housing for low surface temperature
  • Power failure indicator (SPS)
  • Runtime meter (SPS)
  • Countdown timer for each cell (SPS)
  • Alarm history
  • Microfilter for the air that removes 99.99 % of all particles above 0.1 μm

Optional Accessories for Relaxation & Creep Testing

Expand your Elastocon testing system for tensile, compressive, fluid-based, or flexural testing – with perfectly matched accessories for your specific application.

 

🔹 Accessories for Tensile Testing

For converting rigs from compression to tensile mode:

✅ EB 02.02 – Grips for stress relaxation in tension according to ISO 6914
✅ EB 02.03 – 100 N load cell for tension, including adapter – ideal for low-force tensile testing
✅ EB 18-II.01 – Special clamp for creep in tension per ISO 899-1

 

🔹 Accessories for Testing in Fluids

For conducting relaxation tests in liquids:

✅ EB 02.01 – Container and perforated compression plate – for testing in accordance with ISO 3384

 

🔹 Accessories for Flexural Testing

For creep testing in flexure on plastic specimens:

✅ EB 02.29 – Three-point bending fixture for creep in flexure as per ISO 899-2

 

With these accessories, your relaxation and creep testing system becomes even more versatile, standards-compliant, and application-optimized – enabling precise testing in tension, compression, fluid environments, and flexure.